01 / GEOMETRY
Complex tread geometry
Non-foamed molding plaster developed for detailed reproduction of complex tire tread configurations.
TIRE MOLD CASTING
Investment materials for aluminum tire mold casting, developed to reproduce complex tread configurations.
Explore investment materials
01 / TREAD. DETAIL. CONTROL.
01 / GEOMETRY
Non-foamed molding plaster developed for detailed reproduction of complex tire tread configurations.
02 / DETAIL
Precise particle sizing supports a smoother as-cast surface. A surface tension reducer assists in removing trapped air bubbles.
03 / PROCESS
Controlled expansion and shrinkage, with a formulation designed to reduce mold cracking and warping.
02 / INVESTMENT MATERIALS
POWERCAST “T” and MOMENTUM TIRE offer the same investment formulation under PRESTIGE and SPECTRA.

Non-foamed, gypsum-bonded investment molding plaster for aluminum tire mold casting, developed for detailed reproduction of complex tread configurations.
Controlled expansion and shrinkage support mold accuracy. Precise particle sizing and a surface tension reducer help produce smoother as-cast surfaces and remove trapped air bubbles. Available in 22.5 kg plastic-lined sacks and 1 metric ton bulk bags.
Ask about POWERCAST “T”
Non-foamed, gypsum-bonded investment molding plaster for aluminum tire mold casting, developed for detailed reproduction of complex tread configurations.
Controlled expansion and shrinkage support mold accuracy. Precise particle sizing and a surface tension reducer help produce smoother as-cast surfaces and remove trapped air bubbles. Available in 22.5 kg plastic-lined sacks and 1 metric ton bulk bags.
Ask about MOMENTUM TIRE03 / PROCESS STARTING POINTS
Catalog guidance for POWERCAST “T” and MOMENTUM TIRE. Match the process to your mixing equipment, pattern and mold size.
Per 1 kg powder: 500 ml water for automatic vacuum mixing, or 520 ml for conventional mixing. Recommended water temperature: 21–24°C.
The catalog gives an 11-minute total working sequence for both mixing methods. Follow the method-specific mixing and vacuum stages.
Leave undisturbed for 120–150 minutes before burnout. Burnout time depends on mold size; discuss your process with our technical team.
04 / TECHNICAL SUPPORT
Share your aluminum alloy, mold dimensions and mixing method. Our team will help you select the investment and plan the process.
chris@certus-int.com ↗